Morphological and Rheological Characterization of Gold Nanoparticles Synthesized Using Pluronic P103 as Soft Template
Figure 2
Intensity of the UV-Vis absorbance peaks measured at 220, 320, and 540 nm for HAuCl4 (2 mM) and P103 (10 wt.%) aqueous solutions at 30°C.