Research Article
Significant Enhancement of Mechanical and Thermal Properties of Thermoplastic Polyester Elastomer by Polymer Blending and Nanoinclusion
Table 1
Initial formulation (wt.%) of the polymeric blends.
| Experiment # | TPEE G155D | PBT (1200-211M) | IF-168 | IF-1010 | MA | PETG (KN100) | Total |
| 1 | 54.50 | 45.00 | 0.20 | 0.20 | 0.50 | 0.00 | 100.4 | 2 | 74.50 | 25.00 | 0.20 | 0.20 | 0.50 | 0.00 | 100.4 | 3 | 74.50 | 15.00 | 0.20 | 0.20 | 0.50 | 10.00 | 100.4 |
|
|