Research Article
Synthesis and Characterization of Nanocrystalline Ni50Al50−xMox (x = 0–5) Intermetallic Compound during Mechanical Alloying Process
Figure 5
Size changes of NiAl crystal after 128 h of milling for samples with 0, 0.5, 1, 2.5, and 5 at.% Mo.