Research Article

Hydrophobic Coatings Composed by Cubic-Shaped CdO Nanoparticles Grown by a Novel and Simple Microwave Method

Figure 5

FE-SEM images of CdO samples after annealing for 1 hr and 15 min at 450°C.
(a)