Research Article
Spreadability of Ag Layer on Oxides and High Performance of AZO/Ag/AZO Sandwiched Transparent Conductive Film
Table 2
Haacke figure of merit of IAI and ZAZ sandwiched layers.
| Sandwiched layers | , % | , Ω/sq | , Ω−1 |
| ITO (34 nm)/Ag (7 nm)/ITO (34 nm) | 84.87 | 7.79 | 0.02488 | ITO (37 nm)/Ag (7 nm)/ITO (37 nm) | 85.14 | 8.04 | 0.02489 | ITO (34 nm)/Ag (9 nm)/ITO (34 nm) | 78.64 | 5.64 | 0.01604 | ITO (37 nm)/Ag (9 nm)/ITO (37 nm) | 79.73 | 5.53 | 0.02237 | ITO (34 nm)/Ag (11 nm)/ITO (34 nm) | 84.14 | 4.64 | 0.03833 | ITO (37 nm)/Ag (11 nm)/ITO (37 nm) | 83.52 | 4.61 | 0.03583 | ITO (30 nm)/Ag (13 nm)/ITO (30 nm) | 80.21 | 4.23 | 0.02606 | ITO (37 nm)/Ag (13 nm)/ITO (37 nm) | 79.59 | 4.14 | 0.02464 | AZO (25 nm)/Ag (7 nm)/AZO (25 nm) | 83.69 | 5.76 | 0.02926 | AZO (27 nm)/Ag (7 nm)/AZO (27 nm) | 81.39 | 4.82 | 0.02646 | AZO (32 nm)/Ag (9 nm)/AZO (32 nm) | 85.81 | 4.08 | 0.05305 | AZO (35 nm)/Ag (9 nm)/AZO (35 nm) | 85.55 | 3.84 | 0.05469 | AZO (40 nm)/Ag (9 nm)/AZO (40 nm) | 83.88 | 3.67 | 0.04698 | AZO (35 nm)/Ag (11 nm)/AZO (35 nm) | 75.15 | 3.11 | 0.01847 | AZO (40 nm)/Ag (11 nm)/AZO (40 nm) | 77.34 | 3.10 | 0.02470 | AZO (19 nm)/Ag (13 nm)/AZO (19 nm) | 74.45 | 3.03 | 0.01727 | AZO (27 nm)/Ag (13 nm)/AZO (27 nm) | 74.49 | 2.54 | 0.02071 |
|
|