]>Development of SBR-Nanoclay Composites with Epoxidized Natural Rubber as Compatibilizer : Table 2
Table 2: Mechanical properties of the rubber compounds.

Sample codeTensile strength (MPa)Elongation at break (%)100% modulus300% modulusTear strength (N/mm)

SBR1.603930.801.287.60
SBR/5EC2.954521.001.9811.80
SBR/10EC3.004541.032.1013.40