Research Article

Improving the Hydrophobicity of ZnO by PTFE Incorporation

Figure 1

X-ray diffractograms of (a) as-deposited ZnO coating and (b) ZnO coating heat treated at 70°C and immersed in stearic acid (0.002 M).
392754.fig.001a
(a)
392754.fig.001b
(b)