The Optimum Dispersion of Carbon Nanotubes for Epoxy Nanocomposites: Evolution of the Particle Size Distribution by Ultrasonic Treatment

Figure 11

Scanning electron micrographs of the MWCNTs after TGA sample preparation. MWCNTs dispersed 10 min in a bath sonicator (a) and at 70% for 72 min (b).
545930.fig.0011a
(a)
545930.fig.0011b
(b)