The Overall Effects of AlN Nanoparticle Addition to Hybrid Magnesium Alloy AZ91/ZK60A

Table 4

Results of compressive testing of AZ91/ZK60A and AZ91/ZK60A/AlN nanocomposite.

Material0.2% CYS (MPa)UCS (MPa)Failure Strain (%)Energy absorbed,
EA (MJ/m3)a

AZ91/ZK60A 1 0 6 ± 5 5 0 8 ± 1 7 1 9 . 5 ± 1 . 7 8 3 ± 9
AZ91/ZK60A/1.5 vol% AlN 1 0 7 ± 1 2 (+1) 5 4 1 ± 1 9 (+6) 2 4 . 1 ± 6 . 5 (+24) 8 8 ± 7 (+6)

aEnergy absorbed until fracture, that is, area under the engineering stress-strain curve until the point of fracture (obtained using EXCEL software).
() Brackets indicate % change with respect to corresponding result of AZ91/ZK60A.