Properties of Electrospun TiO2 Nanofibers

Table 3

Grain size and phase with changes of temperature.

Temperature (°C)Crystallographic planePhaseGrain size (nm)

400(011)Amorphous5.0

500(011)Anatase8.4
600(011)15.7

700(110)Rutile38.4
800(110)48.1
1000(110)64.2
1200(110)71.0
1400(110)613.0