Research Article
[Retracted] Corrosion Inhibition of Tubing Steel during Acidization of Oil and Gas Wells
Table 2
Corrosion parameters in absence and in presence of AAL and BAL at different temperatures.
| Temperature (K) | Blank | AAL | BAL | CR (mpy) | IE% | CR (mpy) | IE% | CR (mpy) | IE% |
| 298 | 9.55 | — | 1.70 | 82.2 | 0.93 | 90.2 | 303 | 12.09 | — | 2.63 | 78.2 | 1.79 | 85.1 | 313 | 19.27 | — | 4.87 | 74.7 | 4.21 | 78.1 | 323 | 30.42 | — | 10.51 | 65.4 | 9.01 | 70.3 | 333 | 48.94 | — | 20.09 | 58.9 | 18.31 | 62.5 |
|
|