Research Article

Thermolysis of High-Density Polyethylene to Petroleum Products

Table 1

Composition of gas products obtained from pyrolysis of polyethylene at 400°C [1].

ComponentThermalCatalyticHydrocracking

Methane22.712.421.1
Ethane27.420.421.2
Ethylene1.42.30.1
C326.630.423.7
C411.020.320.7
C56.95.67.3
C62.13.33.8