Research Article

Poly(acrylonitrile-co-butadiene-co-styrene) Reinforced with Hollow Glass Microspheres: Evaluation of Extrusion Parameters and Their Effects on the Composite Properties

Figure 1

(a) HGM incorporation at the feeding zone with 2.5, 5.0, and 7.5 wt.% HGM + ABS incorporated at Z1; (b) incorporation of HGM at the central extruder zone (Z2) with 2.5, 5.0, and 7.5 wt.% HGM and ABS incorporated at Z1.
(a)