Research Article
Improvement of the Contact Strength of Al2O3/SiC by a Combination of Shot Peening and Crack-Healing
Table 2
Surface roughness of each test specimen.
| Specimens | Maximum height roughness (m) |
| Smooth | 0.445 | SP | 0.498 | SP + CH (950°C for 100 h) | 0.471 | SP + CH (950°C for 100 h) Nonpolishing | 0.530 | CH (1300°C for 1 h) | 0.554 |
|
|