Review Article
Recent Progress in Processing of Tungsten Heavy Alloys
Figure 2
SEM micrograph of two-stage sintered 93W-5.6Ni-1.4Fe WHAs secondarily sintered at 1470°C for (a) 4 min and (b) 90 min after solid-state sintering at 1300°C for 1 h [78].
(a) |