Recent Progress in Processing of Tungsten Heavy Alloys
Figure 3
Longitudinal microstructure of 93W-4.9Ni-2.1Fe alloy samples: (a) as-sintered and (b) hot hydrostatically extruded at an extrusion ratio of 2.86 : 1, respectively [92].