Figure 2: Resistance value variation at room temperature of an In2O3 nanostructured layer. Notice: (a) the resistance diminution in 4 orders of magnitude under illumination, (b) the PPC effect, and (c) the recovery of the initial value after heating for 15 minutes at 325°C.