Schottky Junction Methane Sensors Using Electrochemically Grown Nanocrystalline-Nanoporous ZnO Thin Films

Table 1

The crystal size, pore size, and thickness of the anodized ZnO thin films.

ParametersAnodized ZnO

Crystal size (nm)2.40
Pore size (nm)19–35
Thickness ( m)8.20