Growth and Characterization of Single Crystalline Bi4Ge3O12 Fibers for Electrooptic High Voltage Sensors
Figure 3
Left: schematics of the micro-pulling-down apparatus for BGO fiber growth. Top right: photograph of the platinum crucible. Bottom right: CCD image of the crystallization zone during crystal growth.