Research Article
Damage Detection of Closed Crack in a Metallic Plate Using Nonlinear Ultrasonic Time Reversal Method
Table 2
DI of different paths.
| Number | Path | DI | Number | Path | DI |
| 1 | 2–10 | 0.1982 | 9 | 5–14 | 0.0499 | 2 | 2–13 | 0.0863 | 10 | 6–11 | 0.0302 | 3 | 3–9 | 0.1451 | 11 | 7–9 | 0.1188 | 4 | 3–12 | 0.0965 | 12 | 7–14 | 0.0535 | 5 | 4–12 | 0.0628 | 13 | 7–16 | 0.0345 | 6 | 4–13 | 0.0440 | 14 | 8–12 | 0.0414 | 7 | 4–16 | 0.0459 | 15 | 8–13 | 0.0420 | 8 | 5–10 | 0.1394 | 16 | 8–14 | 0.0503 |
|
|