Research Article
Microoxygraph Device for Biosensoristic Applications
Figure 3
AFM topographic characterization of silver layer. AFM images of untreated silver layer (a); Ag/AgCl layer grown by 0.1 M FeCl3 for 5 min (b) or by 50 mM FeCl3 for 50 sec (c). Scan size, 5 μm.
(a) |
(b) |
(c) |