Research Article

Raman Spectroscopy, X-Ray, SEM, and DTA Analysis of Alkali-Phosphate Glasses Containing and Nb2O5

Table 2

Raman band positions of the LiW-40 and NaW-40 samples and their assignments.

LiW-40NaW-40
Band positionWidth (cm−1)Band position Width (cm−1) Assignment

160.9864.94159.5363.30Deformation
250.81133.03253.69132.79Deformation
377.69112.73382.9380.54Deformation
566.9633.02544.0424.03Deformation
591.6322.08578.0771.09 (Nb-O)
614.6729.68616.7740.38 (Nb-O)
640.6725.74639.7623.78 (Nb-O)- (POP)
764.5290.62763.3986.42 (M-O-P)
834.1972.51843.4482.50 (W-O)
893.1666.56916.0754.02 (Nb-O)/ (W-O)
956.6366.56958.5940.08 (W-O)
979.5084.02 (Nb-O) and/or (W-O)
1017.9274.18 (Nb-O)
1075.2672.501038.15106.63 (PO3)2−
1144.6187.791129.17136.90 (PO2)
1234.0588.501249.2278.98
(PO2) and/or (PO)