XPS, FTIR, EDX, and XRD Analysis of Al2O3 Scales Grown on PM2000 Alloy

Figure 4

XRD powder patterns of as-received PM2000 (a), heat treated on air at 1173 K (b), and heat treated on air from 873 to 1473 K (c).