Research Article
Morphological and Optical Characterization of High Density Au/PAA Nanoarrays
Figure 2
Top view FE-SEM images of (a) PAA membrane pore widened for 70 min and electrodeposited with Au at 5 mA and 57°C for 3 min and PAA membranes pore widened for 60 min and electrodeposited at the same conditions for (b) 4 min and (c) 6 min.
(a) |
(b) |
(c) |