Research Article
The Effective Electrolytic Recovery of Dilute Copper from Industrial Wastewater
Table 1
The copper reduction rate with different types of iron.
| Types of iron | Reduction percent % | 2 h | 4 h | 8 h |
| Without iron | 54.8 | 99 | 99.9 | With ferrous ion | 39.5 | 62.8 | 99.56 | With ferric ion | 28.3 | 46.6 | 83.6 |
|
|