values of different properties of NBB at different firing temperatures (950, 1000, and 1050°C) and percentages of EMHS in soil.

0%10%20%30%40%50%

Weight loss on ignition 0.950.970.960.950.890.96
Shrinkage on ignition 0.810.850.990.980.980.98
Compressive strength0.810.830.80.850.970.68