Research Article

Analysis of a Nondestructive Evaluation Technique for Defect Characterization in Magnetic Materials Using Local Magnetic Measurements

Table 1

Measurements of the magnetic induction B (in Tesla) at 12 points on the surface of the strip for several values of the imposed current and for a defect with α=-0.001 m and β=0.01m.

Needle sensorIset(A)
position (mm) 0.5 1 1.5 2 2.5 3

-34 0.92 1.24 1.33 1.41 1.45 1.49
-24 0.89 1.16 1.13 1.3 1.35 1.39
-14 0.89 1.19 1.22 1.31 1.35 1.35
-4 0.93 1.28 1.35 1.38 1.4 1.46
3.5 0.98 1.45 1.63 1.68 1.72 1.76
6 1.03 1.38 1.45 1.53 1.56 1.59
8.5 0.99 1.41 1.5 1.56 1.62 1.65
11 1.04 1.35 1.44 1.49 1.55 1.58
13.5 0.92 1.27 1.38 1.42 1.48 1.54
16 0.79 1.18 1.32 1.35 1.4 1.51
26 0.8 1.18 1.25 1.3 1.41 1.44
36 0.81 1.17 1.17 1.24 1.42 1.36