Research Article
A Comparative Study of Spin Coated Transparent Conducting Thin Films of Gallium and Aluminum Doped ZnO Nanoparticles
Figure 6
Sheet resistance and optical transmission at 550 nm, of spin coated GZO (a) and AZO (b) multilayers, sintered in air at 600°C and further postannealed in forming gas at 400°C, as a function of layer thickness. Each single layer is approximately 52–55 nm thick.