Summary of MSC differentiation dependence on substrate stiffness.

LineageMatrix stiffness, MaterialTesting methodReference

Neurogenic 0.1–1 kPa2D polyacrylamide gels, collagen coatedNanoindentation using atomic force microscopy[10]
~1 kPa2D polyvinyl alcohol hydrogelCompression test[53]
1 kPa3D type I collagen gel and hyaluronic acid gelCompression test[55]
~1-2 kPa2D gelatin-hydroxyphenylpropionic acid gelDynamic shear deformation 1%, 1 Hz using rheometer[57]
6.1 kPa 2D polyacrylamide gel (PAA)Compression test[54]

Gliogenic 10 kPa3D type I collagen gel and hyaluronic acid gelCompression test[55]

Vascular endothelial cells2-3 kPa3D polyethylene glycol dimethacrylate (PEGdma) nanofiber hydrogelTensile test[61]

2.5–5 kPa3D alginates-agarose hydrogel with RGDCompression test[132]
Adipogenic4 kPa2D polyacrylamide gel (PAA)Nanoindentation using atomic force microscopy[49]
1.5 kPa, 6 kPa2D polydimethylsiloxane (PDMS)Tensile and macroscopic indentation tests[56]

Myogenic7–17 kPa2D polyacrylamide gels (PAA), collagen coatedNanoindentation using atomic force microscopy[10]
12–15 kPa3D polyethylene glycol dimethacrylate (PEGdma) nanofiber hydrogelTensile test[61]
~30 kPa2D gelatin- hydroxyphenylpropionic acid gelDynamic shear deformation 1%, 1 Hz using rheometer[57]
>9 kPa: 25 kPa, 80 kPa2D polyacrylamide gel, coated with collagen, fibronectinDynamic mechanical analysis[22]

Cardiomyocytes45 and 65 kPa3D thermosensitive hydrogel (PAA and HEMA-PTMC)Tensile test[46]

Osteogenic11–30 kPa3D alginates-agarose hydrogel with RGDCompression test[132]
15–100 kPa2D polydimethylsiloxane (PDMS)Tensile and macroscopic indentation tests[56]
24 kPa2D polyvinyl alcohol hydrogelCompression test[53]
25–40 kPa2D polyacrylamide gels, collagen coatedNanoindentation using atomic force microscopy[10]
30 kPa2D polyacrylamide gel (PAA)Nanoindentation using atomic force microscopy[49]
42 kPa2D polyacrylamide gel (PAA) collagen coatedTensile test[78]
46.7 kPa2D polyacrylamide gel (PAA)Compression test[54]
~60 kPa2D gelatin–hydroxyphenylpropionic acidDynamic shear deformation 1%, 1 Hz using rheometer[59]
80 kPa2D polyacrylamide gel
coated with collagen, fibronectin
Dynamic mechanical analysis[22]
190 kPa–3.1 MPa2D polydimethylsiloxane (PDMS)Nanoindentation[58]