Table 1:
Amount of attached HRP protein (determined from FTIR ATR using (
5
)) on UHMWPE treated by PIII with 20 keV energy Nitrogen ions at 10
16
ions/cm
2
fluence.
Substrate
As attached
Washed in SDS
Untreated
PIII treated, new
PIII treated, after 2 years