Research Article

Multilayer Inorganic Electrets with and Layers for Applications on Heated Machinery

Figure 7

Decrease of the surface potential in the ON-2-type electret caused by a sequential anneal for 10 min at different temperatures, from room temperature (RT) to 450°C. Before the experiment, the sample was discharged in the water from left and right for 6-7 mm.
904168.fig.007