Research Article
The Effects of Salt on Rheological Properties of Asphalt after Long-Term Aging
Table 3
Failure temperature after PAV of conventional bitumen soaked in saline water.
| Conventional bitumen | 0% 0 d | 0.3% 1 d | 0.3% 30 d | 1% 1 d | 1% 7 d | 3% 7 d | 3% 15 d | 5% 15 d | 5% 30 d |
| Failure temperature (°C) | 73.10 | 73.44 | 73.49 | 73.42 | 74.02 | 73.88 | 74.69 | 74.09 | 74.43 |
|
|