Research Article

Effect of Repeated Thermal Shock on Mechanical Properties of ZrB2-SiC-BN Ceramic Composites

Figure 2

Temperature curve of a single thermal shock: (a) 1200°C; (b) 1400°C; (c) 1600°C; (d) 1800°C.
419386.fig.002a
(a)
419386.fig.002b
(b)
419386.fig.002c
(c)
419386.fig.002d
(d)