Figure 4

Residual strengths of ZSB materials after thermal shock for different times: (a) 1200°C; (b) 1400°C; (c) 1600°C; (d) 1800°C.
419386.fig.004a
(a)
419386.fig.004b
(b)
419386.fig.004c
(c)
419386.fig.004d
(d)