Research Article
Effect of Zirconium Oxide Nanofiller and Dibutyl Phthalate Plasticizer on Ionic Conductivity and Optical Properties of Solid Polymer Electrolyte
Table 1
Conductivity values of SPE at ambient temperature.
| Sample | Conductivity | (Scm−1) |
| PEO | 1.58 × 10−9 | PEO + 4 wt.% LiCF3SO3 | 4.17 × 10−8 | PEO + 8 wt.% LiCF3SO3 | 4.91 × 10−7 | PEO + 12 wt.% LiCF3SO3 | 1.37 × 10−6 | PEO + 14 wt.% LiCF3SO3 | 9.24 × 10−6 | PEO + 14 wt.% LiCF3SO3 + 1 wt.% DBP | 4.51 × 10−5 | PEO + 14 wt.% LiCF3SO3 + 5 wt.% DBP | 4.96 × 10−6 | PEO + 14 wt.% LiCF3SO3 + 10 wt.% DBP | 5.94 × 10−6 | PEO + 14 wt.% LiCF3SO3 + 15 wt.% DBP | 6.20 × 10−6 | PEO + 14 wt.% LiCF3SO3 + 20 wt.% DBP | 7.73 × 10−6 | PEO + 14 wt.% LiCF3SO3 + 1 wt.% DBP | 1.38 × 10−4 | + 0.05 wt.% ZrO2 | PEO + 14 wt.% LiCF3SO3 + 1 wt.% DBP | 4.71 × 10−5 | + 0.10 wt.% ZrO2 | PEO + 14 wt.% LiCF3SO3 + 1 wt.% DBP | 4.96 × 10−5 | + 0.50 wt.% ZrO2 | PEO + 14 wt.% LiCF3SO3 + 1 wt.% DBP | 4.98 × 10−5 | + 1.00 wt.% ZrO2 |
|
|