Research Article
Structural, Optical, and Magnetic Properties of NiMoO4 Nanorods Prepared by Microwave Sintering
Figure 2
(a) XRD patterns of the as-prepared powder and the powders heated at 600°C for 10 minutes in a microwave oven together with (b) structural refinements plot for the α,β-NiMoO4 nanostructures.
(a) |
(b) |