Research Article

Structural, Morphological, and Electron Transport Studies of Annealing Dependent In2O3 Dye-Sensitized Solar Cell

Table 3

Photovoltaic parameters of In2O3 thin film annealed at 350°C, 450°C, and 550°C.

Annealing
temperature (°C)
(V) (mA/cm2)FF (%)

3500.352.50.320.28
4500.429.20.431.54
5500.365.80.350.73