Research Article
Wear Behavior of Aluminium Metal Matrix Composite Prepared from Industrial Waste
Figure 11
(a) SEM of worn surface of sample-II after running 2000 m at 29.43 N load and 4.71 m/s sliding speed. (b) XRD test report of the worn surface of sample-II.
(a) |