Research Article

Surface Characteristics and High Cycle Fatigue Performance of Shot Peened Magnesium Alloy ZK60

Figure 1

Section topographies of the peened ZK60 alloy at different Almen intensities: (a) 0.05 mmN; (b) 0.10 mmN; (c) 0.30 mmN; (d) 0.40 mmN.
682191.fig.001a
(a)
682191.fig.001b
(b)
682191.fig.001c
(c)
682191.fig.001d
(d)