Research Article

The Effect of Microstructure on Stress-Strain Behaviour and Susceptibility to Cracking of Pipeline Steels

Figure 4

Microstructures of the longitudinal section of the grade X100 air cooled after 30 min. at (a) 600°C and (b) 700°C.
638290.fig.004a
(a)
638290.fig.004b
(b)