Research Article
Cure Cycle Effect on High-Temperature Polymer Composite Structures Molded by VARTM
Table 2
Some cases used to produce composite panel by VARTM.
| Case number | Maximum cure temperature (°C) | Heating rate (°C/min) | Postcure time at 227°C (h) |
| Case 1 | 194 | 1.39 | 2 | Case 2 | 194 | 0.56 | 2 | Case 3 | 183 | 1.39 | 2 | Case 4 | 205 | 1.39 | 2 |
|
|