Research Article

Self-Healing of Ionomeric Polymers with Carbon Fibers from Medium-Velocity Impact and Resistive Heating

Figure 5

Thermal image results of resistive heating experiment. The sample is heated at 1.2 W (row 1), 2.6 W (row 2), and 7.2 W (row 3). Test duration increases from at left to  s at right, in 15 s intervals.
271546.fig.005