Research Article

Direct Fabrication of Cobalt Oxide Nanoparticles Employing Sucrose as a Combustion Fuel

Figure 5

XRD patterns of nanocrystalline Co3O4 samples obtained via F/O molar ratio of 0.5 at different calcination temperature: (a) 350, (b) 400, (c) 500, (d) 600, (e) 700, (f) 800, (g) 900, and (h) 1000°C.
384350.fig.005