Research Article

Effects of Hard Surface Grinding and Activation on Electroless-Nickel Plating on Cast Aluminium Alloy Substrates

Figure 3

Micrographs showing EN deposition on as-received Al alloy substrate after (a) 2 minutes and (b) 10 minutes.
841619.fig.003a
(a)
841619.fig.003b
(b)