Research Article

Localization by Acoustic Emission in Transversely Isotropic Slate

Figure 11

Slate sample B02. The occurrence of new fractures during different phases as observed on crosses and dots are hits localized during these phases, respectively, in the back half or in the front half of the sample. Fractures are drawn as they were observed on the front surface of the sample during testing.
735913.fig.0011a
(a)
735913.fig.0011b
(b)
735913.fig.0011c
(c)
735913.fig.0011d
(d)
735913.fig.0011e
(e)
735913.fig.0011f
(f)
735913.fig.0011g
(g)