(a) Swelling kinetic coefficients of P(DMA-MAx) hydrogels with different MA contents at different pH media. (b) Swelling kinetic coefficients of P(DMA-MA8) hydrogels with different NMBA contents at different pH media.
(a)

MediumHydrogels

pH = 0.9PDMA0.99970.576−3.428
P(DMA-MA8)0.99960.487−3.142
P(DMA-MA15)0.99960.486−3.405
P(DMA-MA29)0.99840.636−4.912
P(DMA-MA33)0.99690.684−4.760
P(DMA-MA38)0.99910.584−4.174

pH = 3.9PDMA0.99980.594−3.997
P(DMA-MA8)0.99930.582−3.762
P(DMA-MA15)0.99890.586−4.209
P(DMA-MA29)0.99780.685−5.263
P(DMA-MA33)0.99860.768−5.242
P(DMA-MA38)0.99920.661−4.615

pH = 6.9PDMA0.99970.559−3.883
P(DMA-MA8)0.99750.553−3.858
P(DMA-MA15)0.99850.582−4.293
P(DMA-MA29)0.99900.553−3.782
P(DMA-MA33)0.99680.661−5.075
P(DMA-MA38)0.99800.650−4.648

pH = 8.7PDMA0.99910.553−3.819
P(DMA-MA8)0.99910.564−3.711
P(DMA-MA15)0.99880.668−4.748
P(DMA-MA29)0.99910.738−5.745
P(DMA-MA33)0.99910.734−5.680
P(DMA-MA38)0.99810.796−5.316

(b)

MediumComposition of NMBA (mol%)

pH = 0.90.160.99760.651−4.617
0.320.99960.487−3.142
0.480.99760.553−3.665
0.640.99640.564−4.021
1.280.99790.523−3.555

pH = 3.90.160.99770.586−4.675
0.320.99930.582−3.762
0.480.99810.589−4.081
0.640.99850.575−4.064
1.280.99680.608−4.410

pH = 6.90.160.99970.606−4.633
0.320.99750.553−3.858
0.480.99740.566−3.858
0.640.99890.571−3.932
1.280.99750.571−4.191

pH = 8.70.160.99840.736−4.974
0.320.99910.564−3.711
0.480.99910.658−4.333
0.640.99710.631−4.178
1.280.99850.687−4.429