Research Article

Nondestructive Investigation of Stress-Induced Damage in Concrete

Figure 6

Surface wave velocity measurements during both the loading and unloading phases of load cycles 2 to 9. The arrows mark the average velocity difference at the stress-free state before and after the application of load in each cycle. The second axis indicates the level of loading as a percentage of the final load at failure.
740189.fig.006