Research Article

Parametric Assessment of Stress Development and Cracking in Internally Cured Restrained Mortars Experiencing Autogenous Deformations and Thermal Loading

Figure 6

(a) Crack opening displacement and (b) average residual stress profile in the reduced strength section of the base case ring specimen when cooled at 48 h.
870128.fig.006a
(a)
870128.fig.006b
(b)