Chemical properties of PC and FA by X-ray fluorescence method.

ā€‰SiO2Al2O3Fe2O3CaOMgONa2OK2OTiO2MnOP2O5SO3LOI

PC [wt.%]20.164.624.5665.351.06ā€”0.440.280.600.072.551.16
FA [wt.%]65.1323.753.381.920.490.481.460.920.070.250.071.65