Research Article
Long Term Compression Strength of Mortars Produced Using Coarse Steel Slag as Aggregate
Table 1
Mortars mix proportions and samples symbolic names.
| | Reference | Chromium oxide | Ultramarine | Aluminium silicate (Na) |
| Cement (g) | 550 | 550 | 550 | 550 | Slag (g) | 1650 | 1650 | 1650 | 1650 | s/c | 0.015 | 0.015 | 0.015 | 0.015 | w/c | 0.36 | 0.36 | 0.36 | 0.36 | Chromium oxide (g) | — | 66 | — | — | Ultramarine (g) | — | — | 66 | — | Aluminium silicate (Na) (g) | — | — | — | 66 |
|
|